The timber is introduced in an airtight chamber where it undergoes an innovative process lasting between 35 and 120 hours, depending on its thickness.

The result is a novel wood product with significantly improved features.

Click on the icons to view description:

 

Proceso Secado Vapor Estabilizacion Enfriamiento


In the initial stage, the wood is rapidly heated up to 100°C.

 